Where do I get good slicer profiles for a filament?

First in this ranking: Bambu Lab PLA Basic.

Ranked filaments

RankFilamentMaterialNozzleBedPrice / kgDatasheetBuy
1Bambu Lab PLA BasicA manufacturer starting point, not a universal PLA profile. PLA Basic lists a nozzle of 190–230 °C (374–446 °F), a bed of 35–45 °C (95–113 °F), and drying at 50 °C (122 °F) for 8 h on the Bambu PLA Basic technical data sheet V3.0.PLA
190–230 °C (374–446 °F)
35–45 °C (95–113 °F)
—Datasheet
2Polymaker Polylite PLAPolyLite PLA lists a nozzle of 190–230 °C (374–446 °F), a bed of 25–60 °C (77–140 °F), a print speed of 40–60 mm/s, and drying at 55 °C (131 °F) for 6 h. The bed range is this sheet, which is wider than the Bambu PLA Basic bed.PLA
190–230 °C (374–446 °F)
25–60 °C (77–140 °F)
—Datasheet
3Prusament PLAPrusament PLA from the Open Filament Database. Nozzle 205–225 °C (401–437 °F) and bed 40–60 °C (104–140 °F). Drying is not stored. Use that row when the spool is Prusament, not the Bambu sheet.PLA
205–225 °C (401–437 °F)
40–60 °C (104–140 °F)
——
4Bambu Lab PETG HFThe same rule on a second material. PETG HF lists a nozzle of 230–260 °C (446–500 °F), a bed of 65–75 °C (149–167 °F), drying at 65 °C (149 °F) for 8 h, and print speed up to 300 mm/s. A PLA profile is the wrong start.PETG
230–260 °C (446–500 °F)
65–75 °C (149–167 °F)
—Datasheet

FilamentFacts may earn a commission when you buy through links on this page. As an Amazon Associate we earn from qualifying purchases.

Use the profile that belongs to the spool, then change temperature, flow, and pressure advance only after a test on that spool. A generic PLA preset is a guess until it matches the row below.

Manufacturer sheets

Bambu PLA Basic lists 190–230 °C (374–446 °F) and 35–45 °C (95–113 °F), with drying at 50 °C (122 °F) for 8 h. PolyLite PLA lists 190–230 °C (374–446 °F) and 25–60 °C (77–140 °F), with drying at 55 °C (131 °F) for 6 h and a print speed of 40–60 mm/s. Prusament PLA lists 205–225 °C (401–437 °F) and 40–60 °C (104–140 °F), and drying is not stored. PETG HF is the reminder that a PLA profile does not carry over: 230–260 °C (446–500 °F) and 65–75 °C (149–167 °F). PLA and PETG are the material hubs.

What these threads actually say

The r/FixMyPrint vq9gnz comment we can point at is about Cura wall order on droopy overhangs, not a temperature. The supplied comments on r/3Dprinting 105sfr7 are jokes and are not quoted here as advice. The bank also lists r/BambuLab 14uype2, r/BambuLab 1tr09f9, and r/3Dprinting sedzai. This page does not attribute a profile recipe to those three threads, because the supplied excerpts do not include one.

Calibration after the profile

Flow calibration is pressure advance and flow. Drying comes before you decide a profile is wrong. Filament quality is the case where diameter or a tangle makes every profile look bad. This page does not publish an OrcaSlicer download or a flow percent.

Pros and cons

Pros

  • Each temperature belongs to a named sheet or Open Filament Database row.
  • The first step is a profile you can point at, then a calibration on that spool.

Cons

  • The editorial summary names OrcaSlicer calibration tools. The top comments supplied for these five threads do not mention OrcaSlicer, so this page does not treat that name as something these threads said.
  • Two of the supplied comments are jokes about a spider print. They are not a profile.

Printer considerations

Printer limits

What the community says

The editorial summary says to start from the slicer's built-in or manufacturer profile, then calibrate temperature, flow, and pressure advance per spool, and it names OrcaSlicer. The supplied top comments do not say OrcaSlicer. One comment on r/FixMyPrint vq9gnz guesses that inner-before-outer walls is not enabled in Cura, and the same thread is about droopy overhangs. The r/3Dprinting 105sfr7 comments supplied here are jokes. This page keeps the manufacturer-sheet start, which the catalog can show, and leaves OrcaSlicer as an unverified line in the summary.

Sources & notes

Accessed 16 October 2026.

Answer JSON · Markdown

Related questions

Questions

Do the supplied comments recommend OrcaSlicer?

No. The editorial summary names OrcaSlicer. The top comments in this bank for these five threads do not. One of them is about inner-before-outer walls in Cura. Two are jokes. Start from the manufacturer row, then use the flow guide.

Can one PLA profile cover Bambu, Polymaker, and Prusament?

No. Bambu PLA Basic lists a bed of 35–45 °C (95–113 °F). PolyLite PLA lists 25–60 °C (77–140 °F). Prusament PLA lists 40–60 °C (104–140 °F). Load the row for the spool.