PETG
How do I get good PETG prints?
First in this ranking: Bambu Lab PETG HF.
- Nozzle230–260 °C (446–500 °F)
- Bed65–75 °C (149–167 °F)
- Speedup to 300 mm/s
- Dry65 °C (149 °F) for 8 h
- Density1.28 g/cm³
Ranked filaments
| Rank | Filament | Material | Nozzle | Bed | Price / kg | Datasheet | Buy |
|---|---|---|---|---|---|---|---|
| 1 | Bambu Lab PETG HFBambu PETG HF technical data sheet, checked 15 October 2026. Nozzle 230–260 °C (446–500 °F), bed 65–75 °C (149–167 °F), drying 65 °C (149 °F) for 8 h, print speed up to 300 mm/s. Enclosure required is blank on the row. | PETG | 230–260 °C (446–500 °F) | 65–75 °C (149–167 °F) | — | Datasheet | |
| 2 | Bambu Lab PETG TranslucentNozzle 220–250 °C (428–482 °F) and bed 70–90 °C (158–194 °F) from the Open Filament Database record. The technical data sheet adds drying at 65 °C (149 °F) for 8 h and print speed up to 220 mm/s. Enclosure required is blank. | PETG | 220–250 °C (428–482 °F) | 70–90 °C (158–194 °F) | — | Datasheet | |
| 3 | Bambu Lab PETG MatteNozzle 230–260 °C (446–500 °F) and bed 65–75 °C (149–167 °F), already on the Open Filament Database record. The sheet adds drying at 65 °C (149 °F) for 8 h and print speed under 250 mm/s. The US store page says PETG Matte is not the support to use under PLA. | PETG | 230–260 °C (446–500 °F) | 65–75 °C (149–167 °F) | — | Datasheet | |
| 4 | Creality CR-PETGOpen Filament Database record. Nozzle 230–250 °C (446–482 °F) and bed 50–70 °C (122–158 °F). Drying and enclosure required are not in our sources. | PETG | 230–250 °C (446–482 °F) | 50–70 °C (122–158 °F) | — | — |
FilamentFacts may earn a commission when you buy through links on this page. As an Amazon Associate we earn from qualifying purchases.
Typical catalog ranges for common PETG spools are in the table. Use the row for the exact spool. The community summary's 230–250 °C (446–482 °F) nozzle and 70–85 °C (158–185 °F) bed are labeled as community process in the section below, and they are not a FilamentFacts lab result.
When to choose PETG
PLA is the easier first print. Move to PETG when the part needs more heat tolerance than PLA and you can dry the spool. The side-by-side of two catalog rows is PLA vs PETG. The PLA failure list stays on good PLA prints.
Plate and first layer
The bank's caveat is adhesion, not a temperature. PETG can weld to smooth PEI. Use glue stick or a textured plate. Keep part cooling low, slow the first layer, and raise Z offset slightly if the first layer is digging in. Bed adhesion splits that advice by material. This page does not publish a fan percentage or a Z-offset distance.
Drying
Dry PETG when it pops or strings. Bambu PETG HF, PETG Translucent, and PETG Matte each list drying at 65 °C (149 °F) for 8 h. Creality CR-PETG does not list drying in our sources. The drying guide keeps the community PETG band of 60–65 °C (140–149 °F) separate from those sheet values.
Stringing
Stringing on a dry spool is the stringing guide and then ooze. Do not treat a wet spool as a retraction problem.
Catalog temperatures
Bambu PETG HF lists 230–260 °C (446–500 °F) and 65–75 °C (149–167 °F). Bambu PETG Translucent lists 220–250 °C (428–482 °F) and 70–90 °C (158–194 °F). Bambu PETG Matte lists 230–260 °C (446–500 °F) and 65–75 °C (149–167 °F). Creality CR-PETG lists 230–250 °C (446–482 °F) and 50–70 °C (122–158 °F). ELEGOO PETG, Hatchbox PETG, and Overture PETG each list 220–250 °C (428–482 °F) and 70–90 °C (158–194 °F), and drying is not in our sources for those three. PolyLite PETG lists 220–250 °C (428–482 °F), 70–90 °C (158–194 °F), and drying at 65 °C (149 °F) for 6 h. Enclosure required is blank on every row named here.
What the bank's comments actually are
The gear thread is about wear on a small tooth, and the badge thread is about a radar cover. Neither comment supplies a nozzle temperature. The process on this page is the editorial summary plus the catalog rows.
Pros and cons
Pros
- The first sentence is process. Temperatures stay on the product row.
- The four ranked spools each have a nozzle and a bed in the catalog, and they do not share one bed range.
Cons
- The top comments in this Reddit bank are about a radar badge and a worn gear. They are not a PETG profile.
- Creality CR-PETG has no drying time in our sources. Do not copy the 8 h from the Bambu sheets onto it.
Printer considerations
- Start from the slicer profile for the spool you loaded. The community nozzle band of 230–250 °C (446–482 °F) is not the cell on every row.
- A smooth PEI plate is the surface this consensus tells you to cover with glue stick or to swap for a textured plate. PETG can weld to bare smooth PEI.
- Match the row's nozzle and bed to the printer maximums. A blank enclosure cell is not a yes.
What the community says
The editorial summary for this cluster is to print PETG with low part cooling, a slower first layer, and a slightly higher Z offset, and to dry the spool if it pops or strings. The caveat on the bank is that PETG sticks too hard to smooth PEI, so people use glue stick or a textured plate. The summary also names a nozzle band of 230–250 °C (446–482 °F) and a bed band of 70–85 °C (158–185 °F). Those bands are community process. They are not the catalog cells below. The highest-scored comments we have for this bank are off-topic, so this page does not quote them as settings.
- Community source, r/3Dprinting 1wu7b2b
- Community source, r/FixMyPrint 13dq7qm
- Community source, r/BambuLab 1kplic3
- Community source, r/BambuLab 1c8ico0
Sources & notes
Accessed 15 October 2026.
- Bambu Lab PETG HF technical data sheet datasheet
- Bambu Lab PETG Translucent technical data sheet datasheet
- Bambu Lab PETG Matte technical data sheet datasheet
- Open Filament Database, Creality CR-PETG other
- Community source, r/3Dprinting 1wu7b2b reddit
- Community source, r/FixMyPrint 13dq7qm reddit
- Community source, r/BambuLab 1kplic3 reddit
- Community source, r/BambuLab 1c8ico0 reddit
Related questions
- How do I get good PLA prints?PLA
- Do I need to dry filament, and how?Drying
- How do I fix bed adhesion problems?Troubleshooting
- How do I fix stringing?Troubleshooting
- How do I stop oozing between moves?Troubleshooting
Questions
Is 230–250 °C (446–482 °F) the PETG nozzle range in the table?
No. That band is the community summary. Bambu PETG HF lists 230–260 °C (446–500 °F) and a bed of 65–75 °C (149–167 °F). Bambu PETG Translucent lists 220–250 °C (428–482 °F) and 70–90 °C (158–194 °F). Creality CR-PETG lists 230–250 °C (446–482 °F) and 50–70 °C (122–158 °F). Use the row for the spool you loaded.
Where are drying and stringing?
Drying and stringing have their own pages. Dry the spool when PETG pops or strings, then tune inside the catalog nozzle range. This page does not add a retraction distance.