Comparison

TPU 95A vs TPU 85A

The tiles and the table are the listed numbers. Source wording sits under Sources & notes.

Prusament TPU 95A

Buy

As an Amazon Associate we earn from qualifying purchases.

  • Nozzle220–240 °C
  • Bed55–75 °C
  • Speed—
  • Dry—
  • Density1.22 g/cm³

Bambu Lab TPU 85A

Buy

As an Amazon Associate we earn from qualifying purchases.

  • Nozzle200–250 °C
  • Bed30–35 °C
  • Speedup to 200 mm/s
  • Dry70 °C maximum
  • Density1.18 g/cm³

Side by side

SpecPrusament TPU 95ABambu Lab TPU 85A
MaterialTPUTPU
Nozzle temperature220–240 °C200–250 °C
Bed temperature55–75 °C30–35 °C
Print speed—up to 200 mm/s
Drying—70 °C maximum
Enclosure required——
Chamber temperatureideal 30 °C and maximum 40 °C—
Hardened nozzle——
Spool weight500 g1 kg (1000 g)
Price per kg——
Sources & notes

Prusament TPU 95A lists a nozzle of 220–240 °C and a bed of 55–75 °C. Bambu Lab TPU 85A lists a nozzle of 200–250 °C and a bed of 30–35 °C. 95A is the stiffer of the two Shore A values. Shore hardness is the grade in the product name, not a second temperature.

Comparison JSON · Markdown

Questions

What nozzle temperatures are listed for TPU 95A vs TPU 85A?

Prusament TPU 95A lists 220–240 °C. Bambu Lab TPU 85A lists 200–250 °C.

What bed temperatures are listed for TPU 95A vs TPU 85A?

Prusament TPU 95A lists 55–75 °C. Bambu Lab TPU 85A lists 30–35 °C.