# Recreus PP print settings (nozzle, bed, dry)

Recreus PP prints at 210–240 °C (410–464 °F) nozzle and 80–100 °C (176–212 °F) bed, per Open Filament Database.

Print at 210–240 °C (410–464 °F) nozzle, 80–100 °C (176–212 °F) bed.

Source: Open Filament Database

## Sources & notes

Recreus PP (PP) has a recommended nozzle temperature of 210–240 °C (410–464 °F) and a recommended bed temperature of 80–100 °C (176–212 °F), according to the Open Filament Database (record https://api.openfilamentdatabase.org/api/v1/brands/recreus/materials/PP/filaments/pp/index.json; dataset imported 2026-10-13).

Dataset imported: 2026-10-13. Open Filament Database generation date, not a lab test.

- Material: PP
- Nozzle: 210–240 °C (410–464 °F)
- Bed: 80–100 °C (176–212 °F)
- Dry: not in our current sources
- Print speed: not in our current sources
- Hardened nozzle: not recorded
- Source: https://api.openfilamentdatabase.org/api/v1/brands/recreus/materials/PP/filaments/pp/index.json

## What nozzle temperature does Recreus PP recommend?

Recreus PP lists a recommended nozzle temperature of 210–240 °C (410–464 °F).

## What bed temperature does Recreus PP recommend?

Recreus PP lists a recommended bed temperature of 80–100 °C (176–212 °F).

## What print speed does Recreus PP list?

Print speed and volumetric flow are not in our current sources in the imported sources.

## Does Recreus PP require an enclosure?

An enclosure requirement is not in our current sources. No chamber temperature is listed either.

## Does Recreus PP require a hardened nozzle?

A hardened-nozzle requirement is not in our current sources.

## How should Recreus PP be dried?

Drying temperature and drying time for Recreus PP are not in our current sources.

## What spool weights does Recreus PP come in?

Spool weight is not in our current sources.

## What is the price per kilogram of Recreus PP?

Price per kilogram is not in our current sources.