# FiberThree PA12 print settings (nozzle, bed, dry)

Nozzle 240–270 °C (464–518 °F) · Bed 80–100 °C (176–212 °F)

Print at 240–270 °C (464–518 °F) nozzle, 80–100 °C (176–212 °F) bed.

Source: Open Filament Database

## Sources & notes

FiberThree PA12 (PA12) has a recommended nozzle temperature of 240–270 °C (464–518 °F) and a recommended bed temperature of 80–100 °C (176–212 °F), according to the Open Filament Database (record https://api.openfilamentdatabase.org/api/v1/brands/fiberthree/materials/PA12/filaments/pa12/index.json; dataset imported 2026-10-13).

Dataset imported: 2026-10-13. Open Filament Database generation date, not a lab test.

- Material: PA12
- Nozzle: 240–270 °C (464–518 °F)
- Bed: 80–100 °C (176–212 °F)
- Dry: not in our current sources
- Print speed: not in our current sources
- Hardened nozzle: not recorded
- Source: https://api.openfilamentdatabase.org/api/v1/brands/fiberthree/materials/PA12/filaments/pa12/index.json

## What nozzle temperature does FiberThree PA12 recommend?

FiberThree PA12 lists a recommended nozzle temperature of 240–270 °C (464–518 °F).

## What bed temperature does FiberThree PA12 recommend?

FiberThree PA12 lists a recommended bed temperature of 80–100 °C (176–212 °F).

## What print speed does FiberThree PA12 list?

Print speed and volumetric flow are not in our current sources in the imported sources.

## Does FiberThree PA12 require an enclosure?

An enclosure requirement is not in our current sources. No chamber temperature is listed either.

## Does FiberThree PA12 require a hardened nozzle?

A hardened-nozzle requirement is not in our current sources.

## How should FiberThree PA12 be dried?

Drying temperature and drying time for FiberThree PA12 are not in our current sources.

## What spool weights does FiberThree PA12 come in?

Spool weight is not in our current sources.

## What is the price per kilogram of FiberThree PA12?

Price per kilogram is not in our current sources.